Gr9 Titanium Plate
1.Product introduction:Grade 9 Ti-3Al-2.5V titanium sheet is a titanium alloy made by adding a certain amount of Al and V to pure titanium metal. Gr9 titanium sheet is a commonly used titanium alloy because of its high corrosion resistance and moderate mental strength. Mostly used in marine navigation, industrial production, aerospace, and so on. It also has good weldability and easy cold forming.
2.Delivery time: 5-7 days.
3.Payment terms:T/T or L/C.
Description
Production Introduction
Grade 9 Ti-3Al-2.5V titanium sheet is a titanium alloy made by adding a certain amount of Al and V to pure titanium metal. Gr9 titanium sheet is a commonly used titanium alloy because of its high corrosion resistance and moderate mental strength. Mostly used in marine navigation, industrial production, aerospace, and so on. It also has good weldability and easy cold forming.
Standards
ASTM B265
Application Fields
• Aerospace field
• Navigation
• Industrial manufacturing
• Fitness sports
• Chemical chemical industry
Product Display
GR9 Ti Plate Specification
| Specifications | ASTM B265 / ASME SB265 | |||||
| Size Range Plate | 0.020" - 0.098" | |||||
| Standard | ASTM, ASME and API | |||||
| Finish | Hot rolled plate (HR), Cold rolled Plate (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated) | |||||
| Thickness | 4.0 milimeter – 100 milimeter | |||||
| Hardness | Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc. | |||||
| Specialize | Shim Plate, Perforated Plate. | |||||
| Grade | Titanium Grade 9 (UNS R56320) | |||||
| Form | Rolls, Plain Plate, Shim Plate, Perforated Plate, Chequered Plate |
| H | Al | O | V | Fe | N | C |
|---|---|---|---|---|---|---|
| ≤0.013 | ≤3.5 - 2.5 | ≤0.12 | ≤3.0 - 2.0 | 0.25 | ≤0.02 | 0.10 |
GR9 Ti Plate Mechanical Characteristics
| Yield strength | Ultimate strength | Elongation 2" | |||
|---|---|---|---|---|---|
| MPa | ksi | MPa | ksi | % | |
| Annealed | 621 | 90 | 485 | 70 | 15 |
| Room | 400°F | 200°F | 600°F | |
|---|---|---|---|---|
| Temp | 204°C | 93°C | 316°C | |
| Btu/(ft h °F) | 4.4 | 5.3 | 4.6 | 6.1 |
| W/(m °C) | 7.6 | 9.2 | 8.0 | 10.6 |